How to Fill Asphalt Cracks Before Sealing (The Right Way)

By Devon Moore September 19, 2024 9 min read

Crack filling is the step most homeowners rush through, or skip entirely, before applying driveway sealer. It's also the step that determines whether your sealing job holds up through Ontario winters or starts failing within a season. Getting crack filling right is straightforward once you understand the types of cracks you're dealing with and the right products for each.

Share feedback

In This Article
  1. Why Asphalt Cracks Form in Ontario
  2. Understanding Crack Types and What They Mean
  3. When to Fill Cracks vs. When to Replace
  4. Crack Filler Products: What to Use
  5. Step-by-Step Crack Filling Process
  6. When Professional Crack Filling Makes Sense

Why Asphalt Cracks Form in Ontario

Understanding why cracks form helps you assess their severity and choose the right repair approach. Ontario's climate is particularly harsh on asphalt for a specific set of interconnected reasons.

Thermal Expansion and Contraction

Asphalt expands in summer heat and contracts in winter cold. This expansion and contraction places the asphalt surface under repeated tension, and asphalt, like any material, has a fatigue limit. Over years of cycling, the surface develops tension cracks, usually at right angles to the direction of traffic or in patterns following the stress points in the sub-base beneath.

Freeze-Thaw Infiltration

Once a hairline crack forms, water enters. When that water freezes, it expands by approximately 9%, forcing the crack wider. When temperatures rise again, more water enters the now-wider crack. Ontario's 30–80 annual freeze-thaw cycles mean this process repeats relentlessly, turning hairline cracks into structural failures over a few seasons if left unaddressed.

Sub-Base Movement

Sometimes cracks indicate movement or failure in the compacted aggregate base beneath the asphalt rather than fatigue in the asphalt itself. These cracks tend to be wider, more irregular in shape, and sometimes accompanied by slight height differences (one side higher than the other) across the crack, a sign of differential settling.

Pro Tip: Take photos of cracks before filling them. If the same cracks reappear the following season in the same location with greater width, this may indicate ongoing sub-base movement that crack filler alone won't solve, a professional assessment may be needed.

Understanding Crack Types and What They Mean

Not all cracks are created equal, and diagnosing the type correctly prevents you from applying the wrong solution.

Crack Type Width Appearance Cause
Hairline / Shrinkage Under 3mm Fine lines, often in patterns Normal aging, thermal cycling
Medium / Structural 3–25mm Visible gaps, may follow traffic patterns Freeze-thaw progression, fatigue
Edge Cracks Varies Along driveway perimeter Lack of lateral support, tree roots
Alligator / Fatigue Network pattern Interconnected cracks resembling scales Base failure, overloading
Exact Price · Free Quote

Want your exact driveway sealing price?

Skip the guesswork, we quote your actual driveway, itemized line by line, free and no-obligation. Serving Kitchener, Waterloo, Cambridge & Guelph, with quotes ready within 1 business day.

When to Fill Cracks vs. When to Replace

Crack filling is the right solution for isolated, non-structural cracks. It is not a remedy for base failure or widespread deterioration. Knowing the difference prevents expensive mistakes.

Fill These Cracks

  • Hairline cracks (under 3mm) with no height differential across the crack
  • Medium cracks (3–25mm) with no height differential and isolated locations
  • Edge cracks at the perimeter of the driveway (once any root issues are addressed)
  • Cracks that have been stable in width for one or more seasons

Consider Professional Assessment (May Need Patching or Replacement)

  • Alligator cracking over any significant area, this indicates base failure that crack filler cannot resolve
  • Cracks with height differential across them (one side higher than the other), indicating differential settling
  • Cracks wider than 25mm or deep enough that you can see the sub-base below
  • Any crack that was filled last season and has reappeared at the same location wider than before

"Homeowners sometimes call us after spending money on crack filler and sealer when what they really needed was a section replacement. Filling over alligator cracking or cracks with a height difference is money wasted, those cracks will be back within a season."

- Devon, D&D Home Services Founder
Driveway sealing quote (from $450)Asphalt or interlock, size and condition.

Crack Filler Products: What to Use

Several types of crack filler are available for DIY use. Each has appropriate applications and limitations.

Cold-Pour / Liquid Crack Filler (for cracks under 12mm)

Cold-pour crack fillers come in jugs or squeeze bottles and are ready to use without heating. They're asphalt-based liquids that you pour directly into the crack. They're easy to use, inexpensive, and effective for smaller cracks. They cure by evaporation, so warm, dry weather is important. Use the exact filler and sealer instructions to determine when sealcoating is permitted. Black Jack Speed-Fill 6438 allows coating after one hour only under its stated good-drying conditions; cool or humid conditions can extend that time. This named-product example is not a rule for all liquid fillers.

Trowelable / Paste Crack Filler (for cracks 6–25mm)

For wider cracks, a trowelable filler, thicker in consistency than cold-pour, provides better structural fill. Applied with a trowel or putty knife, it can be leveled flush with the surrounding surface. It's more work than cold-pour but produces a neater finish. The wait depends on the named repair product and compatible sealer. Henry HE175’s preparation instructions give different waits for its named crack repairs and pothole patch; follow both product labels.

Hot-Pour Crack Filler (professional-grade)

Hot-pour rubberized crack filler is the professional standard for durable crack repair. Heated in a specialized melter unit until liquid, it's poured into cracks and bonds extremely well to the asphalt walls. When cured, it remains flexible through temperature changes rather than becoming brittle. This is what professional contractors use and why professional crack filling typically outlasts DIY repairs. Equipment cost makes it impractical for homeowners.

Backer Rod (for wide cracks, over 12mm)

For cracks wider than 12mm, it's not practical or cost-effective to fill the full depth with filler. Instead, a foam backer rod, a cylindrical foam rope available at hardware stores, is inserted into the crack to reduce the fill depth before applying filler on top. This saves material and actually produces a stronger repair by controlling where the filler bonds.

Step-by-Step Crack Filling Process

Follow this sequence for the best results when filling cracks before sealing.

  1. Clean the cracks thoroughly. Use a stiff wire brush to remove loose material, vegetation, and debris from inside the crack. A leaf blower or compressed air is excellent for clearing dust after brushing. Any material left in the crack prevents filler adhesion to the crack walls.
  2. Remove any vegetation. Weeds or grass in cracks must be removed, roots and all where possible. Applying filler over live vegetation is pointless; the plant will grow through it. A targeted weed killer applied a few days before, or manual removal with a crack cleaning tool, works best.
  3. Meet the filler’s preparation conditions. Clean and dry the crack as the label directs; a day without rain alone does not prove readiness. Do not use a heat gun as a general drying shortcut: Speed-Fill explicitly says not to heat the product.
  4. Insert backer rod for wide cracks. For cracks over 12mm wide, push backer rod into the crack to within 6–10mm of the surface. This forms the base for your filler layer.
  5. Apply the selected filler as directed. Use its specified crack-width range, preparation, fill depth and finishing method. Do not assume that every liquid or paste repair shrinks by the same amount or needs an overfull finish.
  6. Finish as the filler label directs. Do not apply a universal five-to-fifteen-minute tooling delay. Speed-Fill calls for filling slightly high to allow for settling and another application for deeper cracks; other products may specify different finishing methods.
  7. Confirm readiness before sealing. Follow the actual filler and sealer labels, including their air and surface temperatures, humidity and rain-free window. Neither 24 hours nor 48 hours is a universal minimum or sufficient wait for every repair.

Pro Tip: Use the filler’s stated fill depth and finishing method, not a fixed ten-percent overfill. Speed-Fill’s β€œslightly higher” instruction is specific to that product and is not a measured shrinkage allowance for all fillers.

When Professional Crack Filling Makes Sense

DIY crack filling with consumer cold-pour products is effective and appropriate for minor to moderate cracking. But there are scenarios where professional crack filling is the better investment.

  • Extensive cracking: If you have more than a few isolated cracks, the time and material cost of DIY crack filling begins to approach the cost of professional service, with inferior product quality.
  • Wanting hot-pour durability: If you want the crack repair to last as long as the seal coat rather than needing refilling next season, hot-pour professional repairs are significantly more durable than consumer cold-pour products.
  • Uncertain about severity: If you're unsure whether cracks indicate base failure or can be repaired with filler, a professional assessment before spending money on DIY products is wise.
  • Combining with sealing: When D&D Home Services performs a professional driveway sealing job, crack assessment and filling is included as part of the complete service, ensuring consistent, professional-grade prep before the sealer goes down.

Key Takeaways

  • βœ“ Ontario freeze-thaw cycles turn hairline cracks into structural problems if not addressed annually.
  • βœ“ Identify crack type first: hairline and medium cracks can be filled; alligator cracking indicates base failure.
  • βœ“ Clean cracks thoroughly before filling, vegetation, debris, and moisture prevent filler adhesion.
  • βœ“ Use backer rod for cracks over 12mm wide to control fill depth and save material.
  • βœ“ Follow the named filler’s fill-depth and finishing instructions; do not assume every cold-pour filler needs the same overfill or tooling delay.
  • βœ“ Wait until the named filler and compatible sealer instructions permit coating; cool or humid weather can extend drying.

Need professional crack filling and sealing in Kitchener, Waterloo, Cambridge, or Guelph? D&D Home Services handles the complete job - from crack assessment through sealing, with commercial-grade products. Get a free quote today.

Sources & References

D&D Home Services
Devon Moore, Operations LeadCo-Founder & Operations Lead, D&D Home Services

Devon Moore is the co-founder and Operations Lead at D&D Home Services, with hands-on experience cleaning hundreds of homes across Kitchener-Waterloo, Cambridge, and Guelph.

Driveway sealing quote (from $450)

Asphalt or interlock, size and condition.

Get My Free Quote

Ready to Seal & Protect Your Driveway?

Sealing season runs through early fall, get your free, itemized quote before the calendar fills up. Serving Kitchener, Waterloo, Cambridge & Guelph.

Request serviceCall Now