Asphalt driveways in Ontario take a beating every winter. Freeze-thaw cycles β where water enters cracks, freezes, expands by 9%, and refreezes repeatedly β gradually destroy even well-maintained asphalt. Fall sealing is the single most effective preventive measure available. Here's why it matters and how to do it right.
How Freeze-Thaw Damage Happens
The process is mechanical and relentless. Small cracks form in asphalt through normal weathering, UV exposure, and traffic over time. When temperatures drop below freezing, any water that has entered these cracks expands as it freezes β about 9% in volume. This expansion forces the crack slightly wider. When it thaws, more water enters. When it freezes again, it expands in the wider crack. Over a single winter with 50β100 freeze-thaw cycles (common in Southern Ontario), small cracks become significant damage.
Left untreated, this process leads to:
- Surface cracking that deepens to the base course
- Alligator cracking (interconnected crack network)
- Pothole formation as base material is displaced
- Edge deterioration where driveway meets lawn
A $350 seal coat prevents the damage that leads to a $4,000β$8,000 driveway replacement.
What Driveway Sealing Actually Does
A quality seal coat performs several functions simultaneously:
- Fills micro-cracks: Coal tar emulsion sealants penetrate into fine surface cracking, sealing water entry points
- Creates a water-resistant surface: The sealed surface sheds water rather than absorbing it
- Protects against UV oxidation: Asphalt contains oils that oxidize and evaporate from UV exposure, causing brittleness; sealant slows this process
- Resists chemical penetration: Oil, gasoline, and de-icing salt damage β sealant creates a protective barrier
- Improves appearance: Freshly sealed asphalt has a uniform, rich dark colour that dramatically improves curb appeal
"A properly sealed driveway is visibly different. The deep, uniform black tells any visitor immediately that this home is well-maintained."
β D&D Home Services Driveway Team
When to Seal Your Driveway in Ontario
The optimal sealing window for Kitchener-Waterloo homeowners:
- Ideal window: Mid-September through mid-October
- Minimum temperature: 10Β°C (50Β°F) during application and for 24 hours after
- Maximum temperature: Avoid applying in direct heat above 32Β°C β sealant dries too quickly
- No rain: Avoid application within 24 hours of expected rain
- Minimum curing time: 24β48 hours before vehicle traffic; 48β72 hours for full cure
The absolute cutoff for fall sealing is typically late October in our region. Once overnight temperatures consistently fall below 5Β°C, sealants won't cure properly and the application will fail.
Crack Filling: The Essential First Step
Sealing over unfilled cracks provides limited protection. Proper crack filling must precede sealing:
- Cracks under 6mm (ΒΌ inch): Can be sealed over directly with a quality sealer
- Cracks 6β19mm (ΒΌβΒΎ inch): Should be filled with hot rubberized crack filler before sealing
- Cracks over 19mm (ΒΎ inch): May indicate base failure β filling is a temporary measure; replacement of the affected area is the proper repair
- Alligator cracking: Indicates base failure; filling and sealing won't address the underlying problem
Important: If your driveway has alligator cracking or areas that flex underfoot, you have a base failure issue that sealing won't fix. Get an assessment before sealing β you may need a partial or full replacement that's better done in fall than spring.
Professional vs. DIY Driveway Sealing
| Factor | DIY | Professional |
|---|---|---|
| Material quality | Consumer-grade latex sealer | Commercial coal tar or asphalt emulsion |
| Application method | Brush or squeegee | Commercial spray/squeegee for uniform coat |
| Surface prep | Home hose rinse | Professional pressure wash + crack fill |
| Longevity | 1β2 years | 3β5 years |
| Cost (150mΒ² driveway) | $80β$150 + time | $350β$600 fully completed |
| Results | Adequate | Significantly better |
How Long Does Sealing Last?
With a professional-grade coal tar emulsion application, expect 3β5 years before resealing is needed. Factors that affect longevity:
- Traffic volume (high turning/parking stress areas wear faster)
- Quality of the original asphalt
- Whether crack filling was thorough before sealing
- Number of freeze-thaw cycles each winter
- Chemical exposure (road salt tracked in from vehicles)
What to Expect from D&D's Driveway Sealing Service
Our Driveway Sealing Process
- β Full pressure wash and clean before sealing β sealing over dirt = failure
- β Crack assessment and hot rubberized filler for cracks >ΒΌ inch
- β Commercial-grade coal tar emulsion sealant β not consumer box store product
- β Two-coat application for maximum durability
- β Clear traffic-free curing period notification
- β Serving Kitchener, Waterloo, Cambridge, and Guelph